Troubleshooting
Issue: Too Much Product on Panel
Cause: Over-applying clear coat to the applicator.
Solution: Use a clean applicator, lightly misted with Slow Moe, and avoid adding more clear coat. Work the applicator over the affected area to absorb the excess clear coat from the panel, ensuring a smooth, even finish.
Issue: Product Separation (Contamination)
Symptoms: The product fails to self-level, resulting in waves, ripples, or small bubbles on the surface.
Solution:
- Remove the product using lacquer thinner to eliminate the imperfections.
- Relocate to a shaded area to allow the panel to cool.
- Clean the surface with a panel prep solution, followed by denatured alcohol to ensure it’s ready for reapplication.
- Reapply the clear coat carefully.
Tip: Before applying the clear coat, use a spray bottle to mist denatured alcohol onto the panel to cool it by 20° to 30°, improving application results.
Issue: Extreme Panel Temperature
- Symptoms: Product does not self-level, leading to waves, ripples, or small bubbles.
- Solution:
- Remove the product using lacquer thinner.
- Move to a shaded area, allowing the panel to cool.
- Clean with panel prep solution, then denatured alcohol.
- Reapply clear coat.
(Tip: Use a spray bottle to mist denatured alcohol on the panel to cool it by 20° to 30° before applying clear coat.)
Issue: Contamination on Cured Clear Coat
Contaminants: Pollen, dust, or similar particles.
Solution:
- If the panel is dry, use a spray wax or waterless wash with a microfiber cloth to gently remove contaminants without damaging the surface.
- For fully cured clear coat (after 5-7 days), lightly buff or sand the affected area and spot apply clear coat as needed to restore a flawless finish.